Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 223 °C | 433 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2100F PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing. WRAS certification in recognized col.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2100F PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing, WRAS certification in recognized colors.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2100F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no l.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem 2100N PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem 2100N PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2100R PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2100R PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2110 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2110R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2200F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2200R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2210 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2210F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2210R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM HU2100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM PW2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Ultem PW2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Vicat Softening Point | 223 °C | 433 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® 420HP PBT 30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade Valox HX420.. |