ExxonMobil EXACT™ 8230 Plastomer for Polymer Modification

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Exxon Chemical
Trade Name EXACT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil EXACT™ 8230 Plastomer for Polymer Modification.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exact 8230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties. It is designed for modification of both polypropylenes and polyethylenes in applications such as injection molding and profile extrusion.Key Features: General purpose modifier for high-flow applications.Excellent toughness.High filler and oil acceptance.High clarity.Offered as free-flowing pellets.Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaAdditive: Thermal Stabilizer This polymer complies with FDA regulation 21 CFR 177.1520 (Olefin polymers), paragraph (c) 3.2c, and may be used as articles or components of articles intended for use in contact with food, except for articles used for packing or holding food during cooking. Finished articles may contact food only under Conditions of Use C through H described in Table 2 of 21 CFR 176.170(c).Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.882 g/cc
0.0319 lb/in³
ISO 1183
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ISO 868
Thermal Properties Metric English Comments
Melting Point 169 °C
336 °F
ISO 11357-3
Vicat Softening Point 42.8 °C
109 °F
at 1000g; ISO 306/A
Brittleness Temperature <= -103 °C
<= -153 °F
ASTM D746