Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 175 °C | 347 °F | 50K/h; DIN EN ISO 306 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Vicat Softening Point | 175 °C | 347 °F | ASTM 1525-00 modified |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® 4704 PC (Europe-Africa-Middle East) High heat resistant polycarbonate copolymer, provides of 165 C at 1.82 MPa. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with bi.. |
|||
Vicat Softening Point | 175 °C | 347 °F | ASTM 1525-00 modified |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem ATX100F PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East) Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea.. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® VIC4311 PBT VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® VX5121 PBT (Europe-Africa-Middle East) VALOX VX5121 is a 15 % glass reinforced PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Vicat Softening Point | 175 °C | 347 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Vicat Softening Point | 175 °C | 347 °F | 50°C/h 50N; ISO 306 |
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by.. |
|||
Vicat Softening Point | 175 °C | 347 °F | 50°C/h 50N; ISO 306 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Vicat Softening Point | 175 °C @Load 5.10 kg |
347 °F @Load 11.2 lb |
ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 MCS I8 Polyamide 6 - Impact Modified Increased impact resistance grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main propert.. |