Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM AUT230 PEI Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Vicat Softening Point | 242 °C | 468 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |