Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 104 °C | 220 °F | ASTM D-1525 |
Plaskolite Optix® CA - 900 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 104 °C | 220 °F | Rate A; ASTM D1525 |
Ravago Manufacturing Americas Hysun™ 678 ASA Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families. Availibility: North America F.. |
|||
Vicat Softening Point | 104 °C | 220 °F | ASTM D1525 |
Ravago Manufacturing Americas Hysun™ 678UV ASA Available in North America Additive: UV Stabilizer Features: Good Impact Resistance and High Heat ResistanceRoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Vicat Softening Point | 104 °C | 220 °F | 120°C/hr, 1 kg; ASTM D1525-B |
Americas Styrenics STYRON™ A-TECH™ 1220 High-Impact Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 1220 advanced technology polystyrene resin is a high impact, high modulus resin for extrusion thermoforming applications. The improved durability of this resin allows potential do.. |
|||
Vicat Softening Point | 104 °C | 220 °F | ASTM D1525 |
Total 680 Polystyrene
(discontinued **) Polystyrene 680 is a medium impact polystyrene developed for the foam extrusion and laminate markets. This polymers impact qualities in conjunction with its high flexural strength allow 680 to be ex.. |
|||
Vicat Softening Point | 104 - 260 °C | 220 - 500 °F | Average value: 228 °C Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Vicat Softening Point | 104 °C @Load 1.00 kg |
220 °F @Load 2.20 lb |
ASTM-D1525 |
Ineos ABS Lustran® ABS 349 Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives. |
|||
Vicat Softening Point | 104 °C | 220 °F | ASTM D1525 |
Techmer ES Electrablend® PPS 06001 Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
Vicat Softening Point | 104 °C | 220 °F | Rate B (120°C/h); ASTM D1525 |
Techmer ES Plastiblend® ABS 8011 Availability: North AmericaForms: PelletsFeatures: PlatableInformation provided by TP Composites, Inc. |
|||
Vicat Softening Point | 104 °C | 220 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ABS 7600B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 104 °C | 220 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ABS 7600B (ELG) Description: Blow Molding Grade, Extra High Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 104 °C | 220 °F | ASTM D1525 |
Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |
|||
Vicat Softening Point | 104 °C | 220 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 900 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |