Ravago Manufacturing Americas Hysun™ 678UV ASA

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hysun™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hysun™ 678UV ASA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Additive: UV Stabilizer Features: Good Impact Resistance and High Heat ResistanceRoHS CompliantForm: PelletsInformation provided by Ravago
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.3 MPa
7000 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 70.3 MPa
10200 psi
ASTM D790
Flexural Modulus 2.24 GPa
325 ksi
ASTM D790
Izod Impact, Notched 3.20 J/cm
6.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
217 °F
Unannealed; ASTM D648
Vicat Softening Point 104 °C
220 °F
ASTM D1525