Ravago Manufacturing Americas Echo® RPPC 20/10 BK Recycled Polypropylene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Echo®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Echo® RPPC 20/10 BK Recycled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Copolymer Polypropylene, Unreinforced, 20 MFI, 10 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 240 %
240 %
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Strength 18.0 MPa
2610 psi
50N; ASTM D790
Flexural Modulus 0.848 GPa
123 ksi
1% Secant; ASTM D790
Izod Impact, Notched 5.33 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
9.99 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C
115 °F
ASTM D648
Vicat Softening Point 59.0 °C
138 °F
ASTM D 1525