Mechanical Properties Metric English Comments
Flexural Strength 70.0 MPa

@Temperature 23.0 °C
10200 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE
Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo..
Flexural Strength 70.0 MPa

@Temperature 275 °C
10200 psi

@Temperature 527 °F
ISO 178
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
Flexural Strength 70.0 MPa

@Temperature 275 °C
10200 psi

@Temperature 527 °F
ISO 178
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
Flexural Strength 70.0 MPa

@Strain 6.00 %
10200 psi

@Strain 6.00 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® TP 142-011 900116 Nylon 6
PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 70.0 MPa

@Temperature 80.0 °C
10200 psi

@Temperature 176 °F
Practical Use (Water Absorption 2.5%); ASTM-D790
Toyobo GLAMIDE® T-521 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 70.0 MPa

@Temperature 23.0 °C
10200 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 70.0 MPa

@Treatment Temp. 250 °C,
Time 3600 sec
10200 psi

@Treatment Temp. 482 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Flexural Strength 70.0 MPa

@Treatment Temp. 200 °C,
Time 3600 sec
10200 psi

@Treatment Temp. 392 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V..
Flexural Strength 70.0 MPa

@Treatment Temp. 220 °C,
Time 3.60e+6 sec
10200 psi

@Treatment Temp. 428 °F,
Time 1000 hour
Four point
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide
Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand ..