Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 115 MPa @Temperature 175 °C |
16700 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Flexural Strength | 115 MPa @Temperature 175 °C |
16700 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Flexural Strength | 115 MPa @Strain 6.00 % |
16700 psi @Strain 6.00 % |
ISO 178 |
Lanxess Durethan® B 40 SK 000000 Nylon 6 PA 6, non-reinforced, injection molding |
|||
Flexural Strength | 115 MPa @Strain 7.00 % |
16700 psi @Strain 7.00 % |
Conditioned; ISO 178 |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
Flexural Strength | 115 MPa @Temperature -40.0 °C |
16700 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.4%); ASTM-D790 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 115 MPa @Temperature -40.0 °C |
16700 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.8%); ASTM-D790 |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 115 MPa @Temperature 175 °C |
16700 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |