Mechanical Properties Metric English Comments
Flexural Strength 103 MPa

@Temperature 23.9 °C
15000 psi

@Temperature 75.0 °F
Dry; 325°F 2500psi and Post-Cure; ASTM D790
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Chopped Molding Compound Reinforced
Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle..
Flexural Strength 103 MPa

@Thickness 1.57 mm
15000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP842 Paper Base Laminate  (discontinued **)
Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0..
Flexural Strength 103 MPa

@Thickness 1.57 mm
15000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP193P Synthetic Fabric
Description: 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temp..
Flexural Strength 103 MPa

@Thickness 1.57 mm
15000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP310E Cotton Fabric
Description: Manufactured with a domestic cotton fabric and phenolic resin. Similar to NP310 with improved moisture resistance and electrical properties. Mechanical properties equivalent to NP310. M..
Flexural Strength 103 MPa

@Thickness 1.57 mm
15000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP315 Cotton Fabric
Description: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should ..
Flexural Strength 103 MPa

@Thickness 1.57 mm
15000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP630 Paper Base Laminate
Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500"