Mechanical Properties Metric English Comments
Flexural Strength 138 MPa

@Temperature 260 °C
20000 psi

@Temperature 500 °F
Dry, Autoclave; ASTM D790
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Flexural Strength 138 MPa

@Temperature 23.9 °C
20000 psi

@Temperature 75.0 °F
Dry; CMC form; ASTM D790
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..
Flexural Strength 138 MPa

@Thickness 6.35 mm
20000 psi

@Thickness 0.250 in
CW
Industrial Laminates/Norplex MC603 Paper Base Laminate  (discontinued **)
Description: MC603 is constructed from electrical grade of kraft paper and a specially modified phenolic resin system, and is designed to be used in tap changers, coil support plates and terminal pa..
Flexural Strength 138 MPa

@Thickness 1.57 mm
20000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP193E Synthetic Fabric
Description: 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temp..
Flexural Strength 138 MPa

@Thickness 1.57 mm
20000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP319 Cotton Fabric Base Laminate
Description: Bleached canvas combined with phenolic resin and graphite lubricant. Better moisture resistance and machining characteristics than NP315.
Flexural Strength 138 MPa

@Thickness 1.57 mm
20000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP615 Paper Base Laminate
Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated ..
Flexural Strength 138 MPa

@Thickness 1.57 mm
20000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP630 Paper Base Laminate
Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500"
Flexural Strength 138 MPa

@Thickness 1.57 mm
20000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP639 Paper Base Laminate
Description: Economical paper reinforced laminate developed with capacity to withstand temperatures to 150° C without blistering. High compressive strength and low moisture absorption.Thickness T..
Copyright © lookpolymers.com All Rights Reserved