Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated surfaces to give the resulting laminate better arc resistance. Intended for applications where electrical and moisture requirements are secondary.Thickness Tested: 0.062", 0.125" and 0.500"
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.45 g/cc

@Thickness 1.57 mm
1.35 - 1.45 g/cc

@Thickness 0.0620 in
ASTM D792
Moisture Absorption at Equilibrium 3.0 %

@Thickness 1.57 mm
3.0 %

@Thickness 0.0620 in
ASTM D229
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80 - 100

@Thickness 1.57 mm
80 - 100

@Thickness 0.0620 in
ASTM D785
Tensile Strength, Yield 57.9 MPa

@Thickness 1.57 mm
8400 psi

@Thickness 0.0620 in
CW; ASTM D638
86.2 MPa

@Thickness 1.57 mm
12500 psi

@Thickness 0.0620 in
LW; ASTM D638
Modulus of Elasticity 6.89 GPa

@Thickness 1.57 mm
1000 ksi

@Thickness 0.0620 in
CW; ASTM D229
8.27 GPa

@Thickness 1.57 mm
1200 ksi

@Thickness 0.0620 in
LW; ASTM D229
Flexural Strength 96.5 MPa

@Thickness 1.57 mm
14000 psi

@Thickness 0.0620 in
CW; ASTM D790
138 MPa

@Thickness 1.57 mm
20000 psi

@Thickness 0.0620 in
LW; ASTM D790
Compressive Strength 124 MPa

@Thickness 12.7 mm
18000 psi

@Thickness 0.500 in
ASTM D695
Shear Strength 81.4 MPa

@Thickness 15.7 mm
11800 psi

@Thickness 0.620 in
ASTM D732
Izod Impact, Unnotched 0.304 J/cm

@Thickness 12.7 mm
0.570 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
0.315 J/cm

@Thickness 12.7 mm
0.590 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Flammability, UL94 HB

@Thickness 1.57 mm
HB

@Thickness 0.0620 in
Electrical Properties Metric English Comments
Dielectric Constant 6.49

@Thickness 1.57 mm
6.49

@Thickness 0.0620 in
Permittivity, Cond D-24/23; ASTM D150
Dielectric Strength 27.6 kV/mm

@Thickness 1.57 mm
700 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Dielectric Breakdown 55000 V

@Thickness 1.57 mm
55000 V

@Thickness 0.0620 in
Cond A; ASTM D229 S/S
Dissipation Factor 0.096

@Thickness 1.57 mm
0.096

@Thickness 0.0620 in
Cond D-24/23; ASTM D150
Arc Resistance 110 sec

@Thickness 3.17 mm
110 sec

@Thickness 0.125 in
ASTM D495
Descriptive Properties Value Comments
Bond Strength 1400 lb
0.5", ASTM D229
Color Natural