Material Notes:
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
Silicone Property; Arlon SQA-TMS-024
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
Silicone Property; ASTM D2240
Tensile Strength 5.79 MPa
840 psi
Silicone Property; ASTM D412
Elongation at Break 130 %
130 %
Silicone Property; ASTM D412
Tear Strength 15.8 kN/m
90.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color White