Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer UBE
Trade Name UBEPOL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high melting point and crystallinity, and high cis-1,4-polybutadiene rubber matrix. UBEPOL-VCR is improved on the processability and a lot of physical properties of the conventional polybutadiene rubber (BR).Information provided by UBE.
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
ASTM D412
Tensile Strength at Break 18.6 MPa
2700 psi
ASTM D412
Elongation at Break 460 %
460 %
ASTM D412
100% Modulus 0.00290 GPa
0.421 ksi
ASTM D412
200% Modulus 0.00710 GPa
1.03 ksi
ASTM D412
300% Modulus 0.0121 GPa
1.75 ksi
ASTM D412
Tear Strength 52.0 kN/m
297 pli
ASTM D2240
Users viewing this material also viewed the following: