Material Notes:
This product was developed for one shot airbag covers with improved stiffness and low temperature resistance. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Melt Flow 5.4 g/10 min
5.4 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
10 sec; ASTM D-2240
Tensile Strength, Ultimate 9.20 MPa
1330 psi
ASTM D412
Elongation at Break 505 %
505 %
ASTM D412
Flexural Strength 5.00 MPa
725 psi
ASTM D790
Flexural Modulus 0.165 GPa
23.9 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 54.0 kN/m
308 pli
ASTM D624