Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 50.8 kN/m | 290 pli | Die B, no post cure- press cured for 5 minutes; ASTM D624 |
Multibase SILASTIC® 7-4860 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 50.8 kN/m | 290 pli | ASTM D412 |
Multibase TPSiV™ 3040-85A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 50.8 kN/m | 290 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 50.8 kN/m | 290 pli | ASTM D624 |
Huntsman KRYSTALFLEX® PE 900 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Tear Strength | 50.8 kN/m | 290 pli | ASTM D624 |
Multibase Multi-Flex® D 4201 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone Resistant General Purpose Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInformation p.. |
|||
Tear Strength | 50.8 kN/m | 290 pli | Die B, no post cure; ASTM D624 |
Multibase C6-560 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 50.8 kN/m | 290 pli | ASTM D624 |
Multibase Multi-Flex® A 8620 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automotive Interior PartsCoverings, ProtectiveInformation provide.. |
|||
Tear Strength | 50.8 kN/m | 290 pli | ASTM D624 |
Multibase Multi-Flex® D 3604 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Tear Strength | 50.8 kN/m | 290 pli | ADM D470 |
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Tear Strength | 50.8 kN/m | 290 pli | Die C; ASTM D624 |
Lubrizol Estane® AG 4350 Thermoplastic Polyurethane Type: Estane® AG 4350 is a polyether based aliphatic polyurethane specifically formulated to be used as an adhesive interlayer without the need for a glass surface primer. This polymer is designed.. |
|||
Tear Strength | 50.8 kN/m | 290 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 50.8 kN/m | 290 pli | |
Dow Corning C6-560 LIQUID SILICONE RUBBER KIT Dow Corning® Class VI Elastomers are heat cured elastomer raw materials for use by customers fabricating medical devices and parts.Information provided by Dow Corning |
|||
Tear Strength | 50.8 kN/m | 290 pli | |
Dow Corning SILASTIC® 7-4860 BIOMEDICAL GRADE LSR, KIT Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning |
|||
Tear Strength | 50.8 kN/m | 290 pli | ISO 34-1 |
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 50.8 kN/m | 290 pli | ISO 34-1 |
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 50.8 kN/m | 290 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3975 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti.. |
|||
Tear Strength | 50.8 kN/m | 290 pli | ASTM D470 |
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |