Polymer Property : Tear Strength = 50.8 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 50.8 kN/m
290 pli
Die B, no post cure- press cured for 5 minutes; ASTM D624
Multibase SILASTIC® 7-4860 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tear Strength 50.8 kN/m
290 pli
ASTM D412
Multibase TPSiV™ 3040-85A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
Tear Strength 50.8 kN/m
290 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 50.8 kN/m
290 pli
ASTM D624
Huntsman KRYSTALFLEX® PE 900 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Tear Strength 50.8 kN/m
290 pli
ASTM D624
Multibase Multi-Flex® D 4201 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Heat StabilizedOzone Resistant General Purpose Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInformation p..
Tear Strength 50.8 kN/m
290 pli
Die B, no post cure; ASTM D624
Multibase C6-560 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 50.8 kN/m
290 pli
ASTM D624
Multibase Multi-Flex® A 8620 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automotive Interior PartsCoverings, ProtectiveInformation provide..
Tear Strength 50.8 kN/m
290 pli
ASTM D624
Multibase Multi-Flex® D 3604 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P..
Tear Strength 50.8 kN/m
290 pli
ADM D470
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Tear Strength 50.8 kN/m
290 pli
Die C; ASTM D624
Lubrizol Estane® AG 4350 Thermoplastic Polyurethane
Type: Estane® AG 4350 is a polyether based aliphatic polyurethane specifically formulated to be used as an adhesive interlayer without the need for a glass surface primer. This polymer is designed..
Tear Strength 50.8 kN/m
290 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 50.8 kN/m
290 pli
Dow Corning C6-560 LIQUID SILICONE RUBBER KIT
Dow Corning® Class VI Elastomers are heat cured elastomer raw materials for use by customers fabricating medical devices and parts.Information provided by Dow Corning
Tear Strength 50.8 kN/m
290 pli
Dow Corning SILASTIC® 7-4860 BIOMEDICAL GRADE LSR, KIT
Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning
Tear Strength 50.8 kN/m
290 pli
ISO 34-1
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tear Strength 50.8 kN/m
290 pli
ISO 34-1
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tear Strength 50.8 kN/m
290 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-3975 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti..
Tear Strength 50.8 kN/m
290 pli
ASTM D470
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Copyright © lookpolymers.com All Rights Reserved