Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0024525 - 0.0063765 GPa @Temperature 1350 °C, Time 10800 sec |
0.35571 - 0.92485 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories CT-140 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0034335 - 0.0063765 GPa @Temperature 1500 °C, Time 10800 sec |
0.49799 - 0.92485 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0034335 - 0.0063765 GPa @Temperature 1350 °C, Time 10800 sec |
0.49799 - 0.92485 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PTA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0034335 - 0.0063765 GPa @Temperature 1500 °C, Time 10800 sec |
0.49799 - 0.92485 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PTA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0034335 - 0.0063765 GPa @Temperature 1500 °C, Time 10800 sec |
0.49799 - 0.92485 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0034335 - 0.0063765 GPa @Temperature 1500 °C, Time 10800 sec |
0.49799 - 0.92485 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0024525 - 0.0063765 GPa @Temperature 110 °C, Time 86400 sec |
0.35571 - 0.92485 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories CT-130 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0024525 - 0.0063765 GPa @Temperature 110 °C, Time 86400 sec |
0.35571 - 0.92485 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HACT-150 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0024525 - 0.0063765 GPa @Temperature 1000 °C, Time 10800 sec |
0.35571 - 0.92485 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HACT-150 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0024525 - 0.0063765 GPa @Temperature 1000 °C, Time 10800 sec |
0.35571 - 0.92485 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HACT-155 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0024525 - 0.0063765 GPa @Temperature 1350 °C, Time 10800 sec |
0.35571 - 0.92485 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories HACT-160 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0024525 - 0.0063765 GPa @Temperature 110 °C, Time 86400 sec |
0.35571 - 0.92485 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HACT-160 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0024525 - 0.0063765 GPa @Temperature 1000 °C, Time 10800 sec |
0.35571 - 0.92485 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |