Mechanical Properties Metric English Comments
Modulus of Rupture 0.0024525 - 0.0063765 GPa

@Temperature 1350 °C,
Time 10800 sec
0.35571 - 0.92485 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories CT-140 Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0034335 - 0.0063765 GPa

@Temperature 1500 °C,
Time 10800 sec
0.49799 - 0.92485 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PT-170 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0034335 - 0.0063765 GPa

@Temperature 1350 °C,
Time 10800 sec
0.49799 - 0.92485 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories PTA-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0034335 - 0.0063765 GPa

@Temperature 1500 °C,
Time 10800 sec
0.49799 - 0.92485 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PTA-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0034335 - 0.0063765 GPa

@Temperature 1500 °C,
Time 10800 sec
0.49799 - 0.92485 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PTA-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0034335 - 0.0063765 GPa

@Temperature 1500 °C,
Time 10800 sec
0.49799 - 0.92485 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PTF-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0024525 - 0.0063765 GPa

@Temperature 110 °C,
Time 86400 sec
0.35571 - 0.92485 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories CT-130 Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0024525 - 0.0063765 GPa

@Temperature 110 °C,
Time 86400 sec
0.35571 - 0.92485 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-150 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0024525 - 0.0063765 GPa

@Temperature 1000 °C,
Time 10800 sec
0.35571 - 0.92485 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-150 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0024525 - 0.0063765 GPa

@Temperature 1000 °C,
Time 10800 sec
0.35571 - 0.92485 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-155 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0024525 - 0.0063765 GPa

@Temperature 1350 °C,
Time 10800 sec
0.35571 - 0.92485 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HACT-160 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0024525 - 0.0063765 GPa

@Temperature 110 °C,
Time 86400 sec
0.35571 - 0.92485 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-160 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0024525 - 0.0063765 GPa

@Temperature 1000 °C,
Time 10800 sec
0.35571 - 0.92485 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-165 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).