Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.004905 GPa @Temperature 110 °C, Time 86400 sec |
0.7114 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories APC-120 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 GPa @Temperature 1400 °C |
0.7114 ksi @Temperature 2550 °F |
|
Chosun Refractories CRMG-S02 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 - 0.008829 GPa @Temperature 1500 °C, Time 10800 sec |
0.7114 - 1.281 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 GPa @Temperature 110 °C, Time 86400 sec |
0.7114 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HSC-15G Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 GPa @Temperature 110 °C, Time 86400 sec |
0.7114 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories M55 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 - 0.007848 GPa @Temperature 1500 °C, Time 10800 sec |
0.7114 - 1.138 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 - 0.007848 GPa @Temperature 1500 °C, Time 10800 sec |
0.7114 - 1.138 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 GPa @Temperature 1500 °C, Time 10800 sec |
0.7114 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories SW83 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 GPa @Temperature 110 °C, Time 86400 sec |
0.7114 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories TCH-175SV Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 - 0.008829 GPa @Temperature 1500 °C, Time 10800 sec |
0.7114 - 1.281 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |