Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of.. |
|||
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of.. |
|||
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 130 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, improved notched impact strength and energy absorption under biaxial impact load, good heat-ageing resistance |
|||
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 130 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, improved notched impact strength and energy absorption under biaxial impact load, good heat-ageing resistance |
|||
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber 30% Glass fiber reinforced; injection molding grade |
|||
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber 30% Glass fiber reinforced; injection molding grade |
|||
Puncture Energy | 6.00 J | 4.43 ft-lb | Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures |
|||
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance |
|||
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance |
|||
Puncture Energy | 6.00 J | 4.43 ft-lb | 50%RH; ISO 6603-2 |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 30 W1 000000 Nylon 6, 30% Glass Fiber PA 6, Injection molding grade, 30% glass fibers, weather stabilized |
|||
Puncture Energy | 6.00 J @Temperature -30.0 °C |
4.43 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 30 W1 000000 Nylon 6, 30% Glass Fiber PA 6, Injection molding grade, 30% glass fibers, weather stabilized |