Mechanical Properties Metric English Comments
Puncture Energy 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of..
Puncture Energy 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of..
Puncture Energy 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 130 H2.0 901510 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, improved notched impact strength and energy absorption under biaxial impact load, good heat-ageing resistance
Puncture Energy 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 130 H2.0 901510 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, improved notched impact strength and energy absorption under biaxial impact load, good heat-ageing resistance
Puncture Energy 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber
30% Glass fiber reinforced; injection molding grade
Puncture Energy 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber
30% Glass fiber reinforced; injection molding grade
Puncture Energy 6.00 J
4.43 ft-lb
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures
Puncture Energy 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance
Puncture Energy 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance
Puncture Energy 6.00 J
4.43 ft-lb
50%RH; ISO 6603-2
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per..
Puncture Energy 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 30 W1 000000 Nylon 6, 30% Glass Fiber
PA 6, Injection molding grade, 30% glass fibers, weather stabilized
Puncture Energy 6.00 J

@Temperature -30.0 °C
4.43 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 30 W1 000000 Nylon 6, 30% Glass Fiber
PA 6, Injection molding grade, 30% glass fibers, weather stabilized
Copyright © lookpolymers.com All Rights Reserved