Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 930 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.41 - 199 GPa
930 - 28900 ksi
Average value: 75.9 GPa Grade Count:30
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Flexural Modulus 6.41 GPa
930 ksi
Epoxy Novolac 27%, Carbon fabric 73%
Epoxy Novolac - Dow Chemical "DEN 438". Carbon fabric - "VCA"
Flexural Modulus 6.41 GPa

@Temperature 175 °C
930 ksi

@Temperature 347 °F
ISO 178
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Flexural Modulus 6.41 GPa
930 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES
LNP THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing 20% Glass Fiber.
Flexural Modulus 6.41 GPa
930 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Asia Pacific)
LNP* THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber.
Flexural Modulus 6.41 GPa
930 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MX85738 PP (Asia Pacific)
LNP* Thermocomp* MX85738 is a compound based on Polypropylene resin containing Glass Fiber.
Flexural Modulus 6.41 GPa
930 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP ZF004 PPE+PS
LNP THERMOCOMP* ZF004 is a compound based on PPE+PS resin containing 20% Glass Fiber.
Flexural Modulus 6.41 GPa
930 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MX85738 PP
LNP* THERMOCOMP* MX85738 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Flexural Modulus 6.41 GPa
930 ksi
Tangent; ASTM D790
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire..
Flexural Modulus 6.41 GPa
930 ksi
ASTM D790
Ecomass® 1080ZB92 Filled Polyamide
Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyExcellent ToughnessInformation provided by Technical Polymers
Flexural Modulus 6.41 GPa
930 ksi
ASTM D790
Ensinger XP-154 Compression Molded PI Compound, 40% Graphite, Premium Grade
The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st..
Flexural Modulus 6.41 GPa
930 ksi
ASTM D790
Aaron Industries AAROPRENE® GFABS 4030 Glass Filled Acrylonitrile-Butadiene Styrene
AAROPRENE® GFABS 4000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Flexural Modulus 6.41 GPa

@Temperature 175 °C
930 ksi

@Temperature 347 °F
ISO 178
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..
Copyright © lookpolymers.com All Rights Reserved