SABIC Innovative Plastics LNP THERMOCOMP MX85738 PP (Asia Pacific)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MX85738 PP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* MX85738 is a compound based on Polypropylene resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Time 86400 sec
0.0010 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 66.0 MPa
9570 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
ASTM D638
Tensile Modulus 7.76 GPa
1130 ksi
50 mm/min; ASTM D638
Flexural Strength 96.0 MPa
13900 psi
ASTM D790
Flexural Modulus 6.41 GPa
930 ksi
ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm
5.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 148 °C

@Thickness 3.20 mm
298 °F

@Thickness 0.126 in
unannealed; ASTM D648