Polymer Property : Flexural Modulus = 9.20 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.01 - 9.20 GPa
1160 - 1330 ksi
Average value: 8.60 GPa Grade Count:3
Overview of materials for Phenolic, Resole, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v..
Flexural Modulus 0.600 - 9.20 GPa
87.0 - 1330 ksi
Average value: 2.60 GPa Grade Count:88
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..