Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.13 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS LNP* Thermodcomp* Noryl_PCN2910 compound is a 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Flexural Modulus | 9.13 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF0067W PPA LNP* THERMOCOMP* UF0067W is a compound based on Polyphthalamide resin containing 30% glass fiber. Added features of this material include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flam.. |
|||
Flexural Modulus | 9.13 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WF006L PBT LNP* THERMOCOMP* WF006L is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
Flexural Modulus | 9.13 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Flexural Modulus | 9.13 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |