Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.10 GPa | 1320 ksi | |
Plastcom SLOVAMID 6 GF 30 FRA 5 PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
PlastiComp Complet® LBF40-PA66 40% Long Basalt Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
LATI LAESTRA G/30 30% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)
(discontinued **) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded
(discontinued **) This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for .. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 10% PTFE/Silicone. Added features include: Electrically Conductive. Wear Resistant, Superior Molding. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Flexural Modulus | 9.08 GPa | 1320 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC LNP* Stat-kon* Lexan_LC1500N compound is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Flexural Modulus | 9.13 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS LNP* Thermodcomp* Noryl_PCN2910 compound is a 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT LNP THERMOCOMP* WF006 is a compound based on PBT resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX95523C PC LNP* STAT-KON* DX95523C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Flexural Modulus | 9.12 GPa | 1320 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® E202G30 PBT, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
Solvay TECHNYL® 2412GM05-D PA66, 38% glass fiber, DRY Description: Polyamid 66, reinforced with 38% of glass fiber and mineral filler, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2412GM05-D is used in all sectors o.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
PlastxWorld CEVIAN® B5526 30% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
Plenco 4349 Phenolic, Granular, Transfer Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
Polyplastics Duranex® 330HR Polybutylene Terephthalate (PBT), Hydrolysis resistant, Heat shock resistant, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | Longitudinal |
Goodfellow Polyethylene Fiber/Polyethylene composite Information provided by Goodfellow. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
Polyplastics Duranex® 3306 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 243 SAN, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Flexural Modulus | 9.09 GPa | 1320 ksi | ISO 178 |
BASF Nypel® 6030G HS DB BK 5830 30% Glass Filled PA6 (Dry) Description: Nypel® 6030G HS DB BK5830 is a 30% glass fiber reinforced, heat stabilized, black pigmented, injection molding compound based on recycled PA6..Application: Nypel® 6030G HS DB BK5830.. |
|||
Flexural Modulus | 9.08 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC LNP LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES (Europe-Africa-Middle East) LNP* Thermocomp* JF006E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
Eurostar Star L PA66 15Y D52 PA66, Carbon Filled, Injection Molded Star L PA66 15Y D52 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 9.10 GPa @Temperature 23.0 °C |
1320 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated. |