Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.70 GPa | 1260 ksi | |
Plastcom SLOVAMID 66 GF 25 FRG 5 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | |
Plastcom SLOVAMID 66 GF 25 FRI 2 PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | STN EN ISO 178 |
Plastcom SLOVAMID® 6 GF 35 LS PA6 reinforced with glass fiber, UV stabilized PA 6 for injection molding, reinforced with 35% glass fiber, UV stabilized, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | STN EN ISO 178 |
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi.. |
|||
Flexural Modulus | 8.70 GPa @Temperature 23.0 °C |
1260 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D203 GF30 FR PBT, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178, ASTM D790 |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
Nilit FRIANYL B63 H-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific) LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2mm/min; ASTM D790 |
Kingfa JH720 G30 30% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP PFN16 PA 6 LNP* LUBRICOMP* PFN16 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 2% MOS2. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP PFN16 PA 6 (Asia Pacific) LNP* Lubricomp* PFL-4216 is a compound based on Nylon 6 resin containing Glass Fiber, MOS2. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFG16 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFG16 is a compound based on PA 66 resin containing Glass Fiber, Graphite. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP LNP THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12 LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ASTM D790 |
Plenco 3303 Phenolic, Granular, Injection Molded Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178-93 |
Wellman EcoLon® MRGF1914-BK1 Nylon 66, 40% Mineral and Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178-93 |
Wellman Wellamid® MRGF25/15 22H-NBK1/WE-1364 40% Mineral/Glass Reinforced Nylon 66 Description: Mineral/Glass Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 462 Glass/Mineral Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry) Description: Ultramid® BG40GM45 HS BK-130 is a pigmented black, heat stabilized, 45 % glass and mineral fiber reinforced polyamide 6 injection molding compound. It possesses a balance of engineerin.. |