Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.79 GPa | 1130 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st.. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b.. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ASTM D790 |
PolyOne Edgetek® AS-40GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS (Asia Pacific) GR 30%. 275F (135C) DTUL. UL94 V-1 rated. Halogen free flame retardant. For electrical construction market. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig.. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over.. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific) LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+PS LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP IF006L PA 6/12 (Asia Pacific) LNP* THERMOCOMP* IF006L is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP IF006L PA6.12 LNP* THERMOCOMP* IF006L is a compound based on Nylon 6/12 resin containing 30% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL HFG300 PPE+PS (Asia Pacific) PPE+PS GF30% filled, FR V-0 |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific) LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ASTM D790 |
Techmer ES HiFill® TPX-HTN-01026 A 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Flexural Modulus | 7.79 GPa | 1130 ksi | ASTM D790 |
Westlake Plastics Norylux™ Modified Polyphenylene Oxide 30% glass filled Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d.. |