Material Notes:
LNP* THERMOCOMP* IF006L is a compound based on Nylon 6/12 resin containing 30% Glass Fiber. Added features of this material include: Low Extractible.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 8.75 GPa
1270 ksi
50 mm/min; ASTM D638
Flexural Strength 206 MPa
29900 psi
ASTM D790
Flexural Modulus 7.79 GPa
1130 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm
11.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 198 °C

@Thickness 3.20 mm
388 °F

@Thickness 0.126 in
unannealed; ASTM D648