Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL HFG300 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL HFG300 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PS GF30% filled, FR V-0
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0030 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 22.9 g/10 min

@Load 5.00 kg,
Temperature 300 °C
22.9 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 98.0 MPa
14200 psi
Type I, 10 mm/min; SABIC - Japan Method
Elongation at Yield 8.0 %
8.0 %
Type I, 10 mm/min; SABIC - Japan Method
Flexural Strength 132 MPa
19100 psi
ASTM D790
Flexural Modulus 7.79 GPa
1130 ksi
ASTM D790
Izod Impact, Notched 0.880 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 21.0 - 42.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 - 23.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 100 °C

@Thickness 6.40 mm
212 °F

@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94
V-0

@Thickness 1.80 mm
V-0

@Thickness 0.0709 in
UL 94
5VA

@Thickness 2.50 mm
5VA

@Thickness 0.0984 in
UL 94
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved