Material Notes:
13% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D955
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 5.20 GPa
754 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
ASTM D648