Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.35 GPa | 486 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 3.35 GPa | 486 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CM5820 PC+ABS (Asia Pacific) Cycoloy CM5820 resin is a Mineral Filled Non-FR PC+ABS blend with high impact, high modulus, good chemical resistance & improved surface aesthetic, designed for hand help device chassis that require.. |
|||
Flexural Modulus | 3.35 GPa | 486 ksi | |
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Flexural Modulus | 3.35 GPa | 486 ksi | ASTM D790 |
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Flexural Modulus | 3.35 GPa | 486 ksi | ASTM D790M |
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12110 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12110 have a cherry-red appearance which tur.. |
|||
Flexural Modulus | 3.35 GPa | 486 ksi | 2mm/min; ISO 178 |
Denka TX-600S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Modulus | 3.35 GPa | 486 ksi | 2mm/min; ASTM D790 |
Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |