Denka TX-600S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene

Category Polymer , Thermoplastic
Manufacturer Denka
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka TX-600S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a good balance of transparency, strength and fluidity (methyl methacrylate butadiene styrene), "TE Series/CL Series," transparent ABS resins with excellent color attributes and tensile strength are available (among others).ApplicationsTX is used for:flat display substratesoptical componentsmiscellaneous goods.TP/TH are used for:food package sheeting as well as in manufacturingelectronic equipment and componentsmiscellaneous goodsTE/CL are for:electronic equipment and componentsinformation equipment componentsAV equipment, etc.
Physical Properties Metric English Comments
Density 1.127 g/cc
0.04072 lb/in³
ISO 1183
Melt Flow 1.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
20 g/10 min

@Load 10.0 kg,
Temperature 220 °C
20 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 87
87
ISO 2039-2
Flexural Strength 120 MPa
17400 psi
ISO 178
Flexural Modulus 3.35 GPa
486 ksi
2mm/min; ISO 178
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179-2
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
ISO 75-2
Vicat Softening Point 101 °C
214 °F
50N; ISO 306
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Haze 0.20 %

@Thickness 2.00 mm
0.20 %

@Thickness 0.0787 in
ISO 14782
Transmission, Visible 92 %

@Thickness 2.00 mm
92 %

@Thickness 0.0787 in
ISO 13468-1