Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure

Category Polymer , Rapid Prototyping Polymer
Manufacturer DSM Somos
Trade Name ProtoTherm™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionDSM Somos® 12110 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12110 have a cherry-red appearance which turns to an orange-red color after thermal treatment.ApplicationSomos® 12110 differentiates itself from other high temperature stereolithography materials by increasing in tensile strength and maintaining decent elongation at break after thermal treatment. This makes the material ideal for many applications in the automotive and aerospace markets where strong parts that can resist high temperatures are needed.Information Provided by DSM Desotech Inc.
Physical Properties Metric English Comments
Density 1.15 g/cc

@Temperature 25.0 °C
0.0415 lb/in³

@Temperature 77.0 °F
Water Absorption 0.28 %
0.28 %
ASTM D570-98
Viscosity 410 cP

@Temperature 30.0 °C
410 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 84.5
84.5
ASTM D2240
Tensile Strength, Yield 57.6 MPa
8350 psi
ASTM D638M
Elongation at Break 5.0 %
5.0 %
ASTM D638M
Modulus of Elasticity 3.43 GPa
497 ksi
ASTM D638M
Flexural Strength 108 MPa
15700 psi
ASTM D790M
Flexural Modulus 3.35 GPa
486 ksi
ASTM D790M
Thermal Properties Metric English Comments
CTE, linear 58.0 µm/m-°C

@Temperature -40.0 - 0.000 °C
32.2 µin/in-°F

@Temperature -40.0 - 32.0 °F
ASTM E831-00
85.5 µm/m-°C

@Temperature 0.000 - 50.0 °C
47.5 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-00
124.4 µm/m-°C

@Temperature 50.0 - 100 °C
69.11 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-00
139.1 µm/m-°C

@Temperature 100 - 150 °C
77.28 µin/in-°F

@Temperature 212 - 302 °F
ASTM E831-00
Deflection Temperature at 0.46 MPa (66 psi) 52.9 °C
127 °F
ASTM D648-98c
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
ASTM D648-98c
Glass Transition Temp, Tg 59.3 °C
139 °F
ASTM E1545-00
Electrical Properties Metric English Comments
Dielectric Constant 3.39

@Frequency 1.00e+6 Hz
3.39

@Frequency 1.00e+6 Hz
ASTM D150-98
3.52

@Frequency 1000 Hz
3.52

@Frequency 1000 Hz
ASTM D150-98
3.54

@Frequency 60.0 Hz
3.54

@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 16.6 kV/mm
422 kV/in
ASTM D149-97a
Descriptive Properties Value Comments
Appearance Liquid
Dp (mm) 0.14
Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2) 75.4
Exposure that gives 0.254mm thickness
Ec (mJ/cm2) 12.2
Critical exposure