Mechanical Properties Metric English Comments
Flexural Modulus 23.5 GPa
3410 ksi
ASTM D790
PolyOne Stat-Tech™ X ST6600-0040 ES FR Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Modulus 23.5 GPa
3410 ksi
ASTM D790
LNP Stat-Kon® OC-1006 Polyphenylene Sulfide, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Flexural Modulus 23.5 GPa

@Temperature 23.0 °C
3410 ksi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac..
Flexural Modulus 23.5 GPa

@Temperature 23.0 °C
3410 ksi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
Flexural Modulus 23.5 GPa

@Temperature 23.0 °C
3410 ksi

@Temperature 73.4 °F
ISO 178
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, ..
Flexural Modulus 23.5 GPa
3410 ksi
ISO 178
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural..
Flexural Modulus 23.5 GPa
3410 ksi
ISO 178
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry)
Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur..
Flexural Modulus 23.5 GPa
3410 ksi
GB/T 9341-2008
Sichuan Deyang Haton® hGC51 PPS / AE Polyphenylene Sulfide
Injection molding, conductiveInformation provided by Sichuan Deyang Chemical Co., LTD
Flexural Modulus 23.51 GPa
3410 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched
LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.