Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.96 GPa | 574 ksi | ASTM D790 |
SABIC Innovative Plastics Cycoloy® C7122 PC+ABS (Asia Pacific) Cycoloy*C7122 is a mineral filled, non-halogenated flame retardant PC/ABS. Good stiffness with balanced flow and impact performance. |
|||
Flexural Modulus | 3.96 GPa | 574 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C7122 PC+ABS (Asia Pacific) Cycoloy*C7122 is a mineral filled, non-halogenated flame retardant PC/ABS. Good stiffness with balanced flow and impact performance. |
|||
Flexural Modulus | 3.96 GPa | 575 ksi | ASTM D790 |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Flexural Modulus | 3.96 GPa | 575 ksi | ASTM D790 |
Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened Nylon 66, 13% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Flexural Modulus | 3.96 GPa | 575 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 3.96 GPa | 575 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1013TL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 3.96 GPa | 575 ksi | ASTM D790 |
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Flexural Modulus | 3.96 GPa | 575 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 05012 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.96 GPa | 574 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp QF002 PA6.10 LNP* Thermocomp* QF002 is a compound based on Nylon 6/10 containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.96 GPa | 574 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA 10% Glass Reinforced PPE+PA Alloy. |
|||
Flexural Modulus | 3.96 GPa | 574 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA (Asia Pacific) GR 10%. Increased stiffness of 200000 psi (3000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: lighting. |
|||
Flexural Modulus | 3.96 GPa | 575 ksi | ASTM D790 |
Clariant Renol PCSP0013WT-192 Polycarbonate, Flame Retardant, UV Stabilized, High Opacity Data provided by Clariant Masterbatches |
|||
Flexural Modulus | >= 3.96 GPa | >= 575 ksi | ASTM D790 |
Buckeye Polymers BP RPP 4010 T NAT Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |