Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrablend® PA6/6 05012

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Conductive
Manufacturer Techmer ES
Trade Name Electrablend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® PA6/6 05012.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.92 g/cc
0.0694 lb/in³
ASTM D792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.17 mm
0.0080 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 3.96 GPa
575 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.2 µm/m-°C
44.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 224 °C
435 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
Unannealed; ASTM D648
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Volume Resistivity 1.0 ohm-cm
1.0 ohm-cm
ASTM D257
Surface Resistance 1.0 ohm
1.0 ohm
ASTM D257
Shielding Effectiveness 70 dB
70 dB
ASTM D4935
Users viewing this material also viewed the following: