Category Polymer , Thermoplastic , Nylon , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GR 10%. Increased stiffness of 200000 psi (3000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: lighting.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Density 1.162 g/cc
0.04198 lb/in³
ASTM D792
Moisture Absorption 0.500 %
0.500 %
50% RH, 24 hrs; ASTM D570
Moisture Absorption at Equilibrium 1.0 %
1.0 %
50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0065 - 0.0085 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0085 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength at Break 88.0 MPa
12800 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 89.0 MPa
12900 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 10 %
10 %
Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 155 MPa
22500 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 3.96 GPa
574 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
0.530 J/cm

@Temperature -30.0 °C
0.993 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.6 - 50.4 µm/m-°C

@Temperature -20.0 - 150 °C
22.0 - 28.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 245 °C

@Thickness 6.40 mm
473 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C

@Thickness 6.40 mm
410 °F

@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 240 °C
464 °F
Rate B/50; ASTM D1525
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical with Impact 50.0 °C
122 °F
UL 746B
UL RTI, Mechanical without Impact 50.0 °C
122 °F
UL 746B
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
UL 94
Electrical Properties Metric English Comments
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten; ASTM D495
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
Users viewing this material also viewed the following: