Oxford Polymers 901-BK Polycarbonate/Polyetherimide Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polyetherimide (PEI)
Manufacturer Oxford Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers 901-BK Polycarbonate/Polyetherimide Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate/Polyetherimide AlloyInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Water Absorption 0.25 %
0.25 %
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 3.28 GPa
475 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Temperature 23.0 °C
1.40 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 182 °C
360 °F
ASTM D648