Mechanical Properties Metric English Comments
Flexural Modulus 6.20528 - 14.9616 GPa

@Temperature -40.0 - 204 °C
900.014 - 2170.03 ksi

@Temperature -40.0 - 400 °F
Average value: 9.58 GPa Grade Count:2
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..