Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.20528 - 14.9616 GPa @Temperature -40.0 - 204 °C |
900.014 - 2170.03 ksi @Temperature -40.0 - 400 °F |
Average value: 9.58 GPa Grade Count:2 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |