Flexural Modulus 6.20528 - 8.27371 GPa

@Temperature 150 - 150 °C
900.014 - 1200.02 ksi

@Temperature 302 - 302 °F
Average value: 9.03 GPa Grade Count:1
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..
Flexural Modulus 6.20528 - 8.27371 GPa

@Thickness 0.500 - 2.50 mm
900.014 - 1200.02 ksi

@Thickness 0.0197 - 0.0984 in
Average value: 9.03 GPa Grade Count:1
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..
Flexural Modulus 6.20528 - 14.9616 GPa

@Temperature -40.0 - 204 °C
900.014 - 2170.03 ksi

@Temperature -40.0 - 400 °F
Average value: 9.58 GPa Grade Count:2
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..