Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.31 GPa | 335 ksi | Tangent; ASTM D790 |
RheTech Products M12P100-01 12% Mica Reinforced Polypropylene, Black Applications: Fan shroudsAir ductsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® MG38U ABS High impact ABS. UL 746C f1 listed. Toughness/rigidity. Good fatigue resistance. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer Improved flow PC with excellent processability and mold release. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Europe-Africa-Middle East) Improved flow PC with excellent processability and mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical and thermal te.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow Polycarbonate, FDA-compliant Feedstocks, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPM1944 PC Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS (Asia Pacific) LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 LNP* FARADEX* PS003E is a compound based on Nylon 6 resin containing 15% Stainless Steel. Added features of this material include: EMI/RFI Shielding. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Nylene® Naxel™ PC35CV Polycarbonate Description: Naxel™ PC35CV is a 12 melt, virgin, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric .. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-UV3-D-[color]-1 Polycarbonate, UV-stabilized, High Flow with Mold Release Polycarbonate, UV-stabilized, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1325L Polycarbonate, UV Stabilized, High Flow, Mold Release Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | |
Kraton® G1702 + PC blend (5/95) Blending KRATON D and G polymers with PC significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Flexural Modulus | 2.31 GPa @Thickness 3.20 mm |
336 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Europe-Africa-Middle East) LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2801Z PPE+HIPS (Asia Pacific) PPE+HIPS Unfilled FR V-0 100C |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Engineered Plastics EP Alloy 510B PC/ABS Alloy Gray. Stiff tough and excellent color stability. Used in housings for computers, printers, copiers and for auto parts such as air ducts and instrument panels. GMP # 002; Ford # WSS585. Propert.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Entec Hylex® P1025L2 HB Polycarbonate Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Blue Information provided by Entec |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Entec Hylex® P1325L1 HB Polycarbonate UV Stabilized, High Flow, Mold Release, Water ClearInformation provided by Entec. |