Diamond Polymers DIAMALOY 1418EF Polycarbonate/Polyester Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 1418EF Polycarbonate/Polyester Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 265 °C
18 g/10 min

@Load 4.76 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.31 GPa
335 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 4.48 J/cm

@Thickness 3.17 mm,
Temperature -22.0 °C
8.39 ft-lb/in

@Thickness 0.125 in,
Temperature -7.60 °F
ASTM D256
7.43 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
13.9 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256