Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.32 GPa | 336 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers PC-1030L Description: Polycarbonate Information provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific) Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5.. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Asia Pacific) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Asia Pacific) High visocisty PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Europe-Africa-Middle East) High viscosity PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP D10006U PC LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | ASTM D790 |
Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature o.. |
|||
Flexural Modulus | 2.31 GPa @Thickness 3.20 mm |
336 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | ASTM D790 |
KYDEX® FST Fully Compliant Aviation Thermoforming Sheet KYDEX® FST meets all fire, smoke and heat release requirements set forth by the Federal Aviation Regulations 25.853 paragraphs (a) and (d) as well as toxicity requirements for ABD0031, BSS7239 an.. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp DP0039 PC LNP* Lubricomp* DP0039 is a Polycarbonate base resin containing PTFE and Silicone lubricants. Characteristics are: Flame Retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP QL004 PA6.10 LNP* LUBRICOMP* QL004 is a compound based on Nylon 6/10 containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER F-1 weathering certified in natural color, specially designed for Pool & Spa applications. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Asia Pacific) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp 5X06476 FP-V (PVDF) LNP* FP-VM-3830 is a compound based on Polyvinylidine Fluoride (PVDF) containing Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.31 GPa | 336 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® TF-0959 T HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.31 GPa | 336 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® TF-0959 T HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed.. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3500 Natural 1050 Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 4500R Description: Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 4502 Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | ASTM D790 |
Solvay Specialty Polymers Supradel® HTS-2400 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2400 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the.. |
|||
Flexural Modulus | 2.32 GPa | 336 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |