Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.83 - 13.2 GPa | 700 - 1920 ksi | Average value: 7.27 GPa Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |