Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.32 - 1.38 g/cc
0.0477 - 0.0499 lb/in³
Average value: 1.35 g/cc Grade Count:8
Linear Mold Shrinkage 0.000500 - 0.00200 cm/cm
0.000500 - 0.00200 in/in
Average value: 0.00118 cm/cm Grade Count:7
Melt Flow 0.200 - 10.0 g/10 min
0.200 - 10.0 g/10 min
Average value: 1.86 g/10 min Grade Count:5
Ash 40.0 %
40.0 %
Average value: 40.0 % Grade Count:3
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88.0 - 105
88.0 - 105
Average value: 99.8 Grade Count:4
Tensile Strength, Ultimate 64.0 - 101 MPa
9280 - 14700 psi
Average value: 86.9 MPa Grade Count:7
Tensile Strength, Yield 65.0 - 107 MPa
9430 - 15500 psi
Average value: 87.8 MPa Grade Count:5
Elongation at Break 1.00 - 4.00 %
1.00 - 4.00 %
Average value: 3.13 % Grade Count:6
Elongation at Yield 2.00 - 3.00 %
2.00 - 3.00 %
Average value: 2.25 % Grade Count:4
Modulus of Elasticity 5.30 - 11.0 GPa
769 - 1600 ksi
Average value: 6.79 GPa Grade Count:5
Flexural Yield Strength 93.0 - 145 MPa
13500 - 21000 psi
Average value: 124 MPa Grade Count:7
Flexural Modulus 6.84 - 10.8 GPa
992 - 1570 ksi
Average value: 9.34 GPa Grade Count:8
Izod Impact, Notched 0.523 - 1.12 J/cm
0.980 - 2.10 ft-lb/in
Average value: 0.733 J/cm Grade Count:8
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 - 112 °C
212 - 233 °F
Average value: 104 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 92.2 - 106 °C
198 - 223 °F
Average value: 98.1 °C Grade Count:6