Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 153 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.05 GPa
153 ksi
Tangent; ASTM D790
RheTech Products P256-01A Polypropylene Copolymer, Black
Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.05 - 12.4 GPa
153 - 1800 ksi
Average value: 9.87 GPa Grade Count:16
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Flexural Modulus 1.05 GPa
153 ksi
2% Secant; 12.5 mm/min; ASTM D790
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo..
Flexural Modulus 1.05 GPa
153 ksi
ASTM D790A
Ineos L40N-00 Polypropylene Impact Copolymer
L40N-00 is a nucleated high flow polypropylene, medium impact copolymer for injection molding applications. This resin exhibits an excellent balance of resin flow and mechanical properties. This res..
Flexural Modulus 1.05 GPa
153 ksi
ASTM D790A
Ineos R35C-02 Polypropylene Random Copolymer
Grade R35C-02 is a high clarity, lubricated random copolymer with a high flow rate. This material is designed for high-speed injection molding of medium- to thin-walled parts requiring excellent cla..
Flexural Modulus 1.05 GPa
153 ksi
ASTM D790
Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 1.05 GPa
153 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE)
Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol..