Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1370 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 9.45 GPa
1370 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (DAM)
Information provided by Ravago.
Flexural Modulus 9.45 GPa
1370 ksi
ASTM Value
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is..
Flexural Modulus 9.47 GPa
1370 ksi
ASTM D790
Plenco 7466 Phenolic, Granular, Transfer Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406..
Flexural Modulus 9.44 GPa
1370 ksi
ASTM D 790
SABIC Innovative Plastics LNP Stat-kon DEF13 PC
LNP* Stat-kon* DEF13 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup..
Flexural Modulus 9.41 GPa
1370 ksi
ASTM D790
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Flexural Modulus 9.44 GPa
1370 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP AFB42 ABS
LNP* THERMOCOMP* AFB42 is a compound based on ABS containing 10% Glass Fiber, 20% Glass Bead.
Flexural Modulus 9.45 GPa
1370 ksi
ASTM D790
Techmer ES Plaslube® J-1/30/TF/13/SI/2 NAT PA66
Flexural Modulus 9.44 GPa
1370 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF006H PA 66
LNP THERMOCOMP* RF006H is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare.
Flexural Modulus 9.48 GPa
1370 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RF006I PA 66
LNP* THERMOTUF* RF006I is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: High Impact.
Flexural Modulus 9.44 GPa
1370 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF006XXZ PA 66
LNP THERMOCOMP* RF006XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber
Flexural Modulus 9.44 GPa
1370 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66
LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare.
Flexural Modulus 9.44 GPa
1370 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RF007SXP PA 66
LNP* THERMOCOMP* RF007SXP is a compound based on Nylon 66 containing 35% Glass Fiber. Added feature of this material includes: Heat Stabilized.
Flexural Modulus 9.44 GPa
1370 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RX02743 PA 66
LNP* Thermocomp* RX02743 is a compound based on Nylon 66 resin containing Glass Fiber.
Flexural Modulus 9.44 GPa
1370 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RX02743 PA 66 (Asia Pacific)
LNP* Thermocomp* RX02743 is a compound based on Nylon 66 resin containing Glass Fiber.
Flexural Modulus 9.48 GPa
1370 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66
LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 9.41 GPa
1370 ksi
ASTM D790
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Flexural Modulus 9.44 GPa
1370 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP WF006H PBT
LNP* THERMOCOMP* WF006H is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare.
Flexural Modulus 9.48 GPa
1370 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOTUF RF006I PA 66
LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Flexural Modulus 9.48 GPa
1370 ksi
ISO 178
SABIC Innovative Plastics LNP Thermotuf RF006I PA 66
LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region...
Flexural Modulus 9.45 GPa
1370 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East)
Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release.
Flexural Modulus 9.44 GPa
1370 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP WF006H PBT (Asia Pacific)
LNP* Thermocomp* WF006H is a compound based on Polybutylene Terephalate resin containing Glass Fiber.
Flexural Modulus 9.47 GPa
1370 ksi
ISO 178
Polyplastics Duranex® 7390W Polybutylene Terephthalate (PBT), Super low warpage, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 9.45 GPa
1370 ksi
DAM; ISO 178
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc..
Flexural Modulus 9.41 GPa
1370 ksi
2.8mm/min; ASTM D790
Asia International Enterprise (Hong Kong) 60G6-33GF Nylon 66, 33% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Flexural Modulus 9.43 GPa
1370 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Verton MV00ASUV_WH9D703 PP
Preliminary data for 50% Long fiber single color pellet filled PPThis data was supplied by SABIC-IP for the Americas region.
Copyright © lookpolymers.com All Rights Reserved